项 目 \ 牌 号
|
XX
|
X
|
N43
|
N42
|
N41
|
DRN-125
|
DRN-120
|
DRN-115
|
DRN-110
|
| Al2O3 % |
≥42
|
≥42
|
≥40
|
≥40
|
≥42
|
≥45 |
≥42 |
≥40 |
≥36 |
| 耐火度 ℃ |
≥1750
|
≥1750
|
≥1730
|
≥1730
|
≥1750
|
||||
| 显气孔率 % |
≤20
|
≤20
|
≤24
|
≤24
|
≤24
|
≤22(24)
|
≤22(24)
|
≤22(24)
|
≤22(24)
|
| 体积密度 g/cm3 |
≥2.15
|
≥2.15
|
≥2.10
|
≥2.15
|
≥2.25
|
2.15~2.35
|
2.00~2.20
|
2.00~2.20
|
2.00~2.20
|
| 常温耐压强度 Mpa |
≥35
|
≥35
|
≥30
|
≥30
|
≥30
|
≥40
|
≥35
|
≥30
|
≥25
|
| 荷重软化温度KD T2℃ |
≥1450
|
≥1450
|
≥1400
|
≥1450
|
≥1450
|
||||
| 重烧线变化率 % |
1400 ℃×4h
±0.2 |
1400 ℃×4h
±0.2 |
1300 ℃×2h
±0.2 |
1350 ℃×2h
±0.2 |
1400 ℃×2h
±0.2 |
1400 ℃×2h
-0.3~0.1 |
1350 ℃×2h
-0.3~0.1 |
1300 ℃×2h
-0.4~0.1 |
1300 ℃×2h
-0.4~0.1 |
| 0.2Mpa蠕变率 % (20-50)h |
1250 ℃
≤0.2 |
1200 ℃
≤0.2 |
1150 ℃×50h
≤0.8 |
1200 ℃×50h
≤0.8 |
1250 ℃×50h
≤0.8 |
1250 ℃×50h
≤0.8 |
1200 ℃×50h
≤0.8 |
1150 ℃×50h
≤0.8 |
1100 ℃×50h
≤0.8 |
| 使用部位 |
热风炉大墙及格子、蓄热室、燃烧室、混风室墙和底及连络管和各种烧咀砖 |
||||||||